Skip to search boxSkip to navigationSkip to main content

Zero-charge” SiO2/Al2O3 stacks for the simultaneous passivation of n+ and p+ doped silicon surfaces by atomic layer deposition

  • B. van de Loo
    ,
  • ,
  • G. Dingemans
    ,
  • G.J.M. Janssen
    ,
  • M.W.P.E. Lamers
    ,
  • I.G. Romijn
Output:
Contribution to journal
Article
Academic
Peer-review

Open access

Information

Output type

Output:
Contribution to journal
Article
Academic
Peer-review

Original language

English

Pages from-to (Number of pages)

Pages 450-456

Journal (Volume, Issue Number)

Solar Energy Materials and Solar Cells (Volume 143)

Publication milestones

  • E-pub ahead of print - 12/2015
  • Published - 2015

Publication status

Published - 2015

ISSN

0927-0248

Abstract

To achieve high conversion efficiencies, advanced silicon solar cell architectures such as interdigitated back contact solar cells demand that defects at both the n+ and p+ doped Si surfaces are passivated simultaneously by a single passivation scheme. In this work, corona charging experiments show that the fixed charge density Qf is a key parameter governing the passivation of both surface types. Alternatively, Qf can be controlled from strongly negative to even positive values by carefully tuning the SiO2 interlayer thickness in SiO2/Al2O3 stacks prepared by atomic layer deposition (ALD). This control in Qf allows for a superior passivation of n+ Si surfaces by SiO2/Al2O3 stacks compared to a single layer Al2O3. For instance, for SiO2 interlayer thicknesses of ~3–14 nm, the recombination parameter of an n+ Si surface having a high surface doping concentration Ns of 2×1020 cm−3 was reduced from J0n+=81 fA/cm2 to J0n+=50 fA/cm2. Simulations predict that the SiO2/Al2O3 stacks outperform Al2O3 passivation layers particularly on n+ Si surfaces having a moderate Ns in the range of 1018–1020 cm−3. On p+ Si surfaces, J0p+≤54 fA/cm2 was achieved for all ALD SiO2 interlayer thicknesses investigated (i.e., 1–14 nm). The SiO2/Al2O3 stacks presented in this work are compatible with SiNx capping and subsequent high-temperature firing steps, which are typically used in solar cell processing. Furthermore, the results were successfully reproduced in an industrial ALD batch reactor using a low-temperature process. This makes ALD SiO2/Al2O3 stacks a promising candidate for the simultaneous passivation of n+ and p+ Si surfaces in solar cells.

Documents and Links

Metrics

Metrics

SciVal
FWCI
0.97
SciVal
Author count
8
SciVal
Paper percentile
70
SciVal
citations
30
Download statistics
Download count
638
Scopus
citations
30

PlumX, opens in new tab

Captures
47
Citation count
31