On the kinetics of spatial atomic layer deposition

  • ,
  • J. Lieshout, van
    ,
  • A. Illiberi
    ,
  • R. Knaapen
    ,
  • F. Roozeboom
    ,
  • A. Asten, van
Output:
Contribution to journal
Article
Academic
Peer-review

Open access

Information

Output type

Output:
Contribution to journal
Article
Academic
Peer-review

Original language

English

Article number

01A108

Journal (Volume, Issue Number)

Journal of Vacuum Science and Technology A (Volume 31, Issue 1)

Publication milestones

  • Published - 2013

Publication status

Published - 2013

ISSN

0734-2101

Abstract

Spatial atomic layer deposition (ALD) is a promising technology for high deposition rate and high-throughput ALD that can be used for roll-to-roll and large-area applications. In an ideal spatial ALD reactor, the design of the injector should be tuned to the deposition kinetics of the ALD reaction, requiring an in-depth knowledge of the dependencies of the growth per cycle (GPC) on the main kinetic parameters. The authors have investigated the deposition kinetics of spatial ALD of alumina from trimethylaluminum and H2O at atmospheric pressure. A kinetic model was developed, which describes the growth per cycle as a function of the main kinetic parameters. The observation of a vt time dependency in the GPC indicates that precursor diffusion to substrate is rate limiting. Next to a fundamental insight into the kinetics of atmospheric pressure spatial ALD, this model can be used for design optimization of new spatial ALD reactors. Furthermore, the model shows that the maximum alumina deposition rates obtainable with spatial ALD are in the order of several nm/s.

Documents and Links

Metrics

Metrics

Scopus
citations
52
SciVal
citations
52
Download statistics
Download count
979
SciVal
FWCI
1.63
SciVal
Author count
6
SciVal
Paper percentile
83

PlumX, opens in new tab

Captures
105
Citation count
52