Low temperature plasma-enhanced atomic layer deposition of metal oxide thin films
- S.E. Potts,
- W. Keuning,
- ,
- G. Dingemans,
- ,
Output:
Contribution to journal
Article
Academic
Peer-reviewOpen access
Information
Output type
Output:
Contribution to journal
Article
Academic
Peer-reviewOriginal language
EnglishPages from-to (Number of pages)
Pages P66-P74 (9 pages)Journal (Volume, Issue Number)
Journal of the Electrochemical Society (Volume 157, Issue 7)Publication milestones
- Published - 2010
Publication status
Published - 2010
ISSN
0013-4651Abstract
Many reported atomic layer deposition (ALD) processes are carried out at elevated temperatures (>150°C), which can be problematic for temperature-sensitive substrates. Plasma-enhanced ALD routes may provide a solution, as the ALD temperature window can, in theory, be extended to lower deposition temperatures due to the reactive nature of the plasma. As such, the plasma-enhanced ALD of Al2O3, TiO2, and Ta2O5 has been investigated at 25–400°C using [Al(CH3)3], [Ti(OiPr)4], [Ti(CpMe)(OiPr)3], [TiCp*(OMe)3], and [Ta(NMe2)5] as precursors. An O2 plasma was employed as the oxygen source in each case. We have demonstrated metal oxide thin-film deposition at temperatures as low as room temperature and compared the results with corresponding thermal ALD routes to the same materials. The composition of the films was determined by Rutherford backscattering spectroscopy. Analysis of the growth per cycle data and the metal atoms deposited per cycle revealed that the growth per cycle is strongly dependent on the film density at low deposition temperatures. Comparison of these data for Al2O3 ALD processes in particular, showed that the number of Al atoms deposited per cycle was consistently high down to room temperature for the plasma-enhanced process but dropped for the thermal process at substrate temperatures lower than 250°C.
Documents and Links
Final published version, 1.11 MB
Metrics
Metrics
Scopus
citations
177
SciVal
citations
177
Download statistics
Download count
1591
SciVal
FWCI
4.09
SciVal
Author count
6
SciVal
Paper percentile
95
SciVal
Top percentile
5
PlumX, opens in new tab
Captures
193
Social media
60
Citation count
178