Atomic layer deposition of highly transparent platinum counter electrodes for metal/polymer flexible dye-sensitized solar cells
- D. Garcia - Alonso,
- V. Zardetto,
- ,
- F. Rossi, De,
- ,
- T.M. Brown
Output:
Contribution to journal
Article
Academic
Peer-reviewInformation
Output type
Output:
Contribution to journal
Article
Academic
Peer-reviewOriginal language
EnglishArticle number
1300831Pages from-to (Number of pages)
Pages 1300831-1/8 (8 pages)Journal (Volume, Issue Number)
Advanced Energy Materials (Volume 4, Issue 4)Publication milestones
- Published - 2014
Publication status
Published - 2014
ISSN
1614-6832Abstract
Atomic layer deposition (ALD) is used to deposit Pt nanoparticles at low temperature (25–150 °C) to fabricate highly transparent counter electrodes (CEs) for flexible dye-sensitized solar cells (DSCs). The Pt nanoparticles (NPs) are deposited for different number of ALD cycles on indium tin oxide (ITO)/polyethylene naphthalate (PEN) substrates. Rutherford backscattering spectroscopy (RBS) and transmission electron microscopy (TEM) are used to assess the Pt NP loading, density, and size. There is a trade-off between transparency and catalytic activity of the CE, and the best cell performances of back-side-illuminated DSCs (˜3.7% efficiency) are achieved for Pt ALD at temperatures in the range of 100–150 °C, even though deposition at 25 °C is also viable. The best cell produced with ALD platinized CE (100 cycles at 100 °C) outperforms the reference cells fabricated with electrodeposited and sputtered Pt CEs, with relative improvements in efficiency of 19% and 29%, respectively. In addition, these parameters are used to fabricate a large area CE for a sub-module (active area of 17.6 cm2), resulting in an efficiency of 3.1%, which demonstrates the scalability of the process.
Documents and Links
Metrics
Metrics
SciVal
citations
30
Download statistics
Download count
10
SciVal
FWCI
1.32
SciVal
Author count
8
SciVal
Paper percentile
78
Scopus
citations
30
PlumX, opens in new tab
Citation count
30
Captures
56
