Area-selective atomic layer deposition: Role of surface chemistry

Output:
Chapter in Book/Report/Conference proceeding
Conference contribution
Academic
Peer-review

Information

Output type

Output:
Chapter in Book/Report/Conference proceeding
Conference contribution
Academic
Peer-review

Original language

English

Pages from-to (Number of pages)

Pages 39-48 (10 pages)

Publication milestones

  • Published - 01/01/2017

Publication status

Published - 01/01/2017

Publisher

Electrochemical Society, Inc., United States

Publication series

  • Publication series name: ECS Transactions
    ISSN (Print): 1938-6737
    ISSN (Electronic): 1938-5862
    Volume: 80
    Number: 3
978-1-62332-472-8

ISBN (Electronic)

9781607685395

Host publication title

Atomic Layer Deposition Applications 13

Host publication editors

  • Stefan De Gendt
  • Jolien Dendooven
  • Fred Roozeboom
  • Chanyuan Liu
  • Jeffrey W. Elam
  • Oscar van der Straten

Related Event

Title

13th Symposium on Atomic Layer Deposition Applications, ALD 2017- 232nd ECS Meeting

Event type

Conference

Date

01/10/2017 - 05/10/2017

Location

National HarborUnited States

Abstract

Area-selective atomic layer deposition is being considered as the next paradigm shift in device fabrication. Besides semiconductor manufacturing, area-selective ALD presents unique opportunities in catalysis and large-area electronics applications. In this contribution, the results of recently developed area-selective ALD processes for In2O3 and ZnO are revisited. These approaches rely on substratedependent nucleation that originates from chemoselective precursor adsorption. Here, we focus on the role of thermodynamics and kinetics of the surface reactions in enabling area-selective deposition. Thermodynamics and kinetics of reactions were calculated by density functional theory (DFT) methods. We believe that our findings can be valuable in understanding area-selective ALD processes at a molecular level, the mechanisms underpinning the chemoselective adsorption and thus in advancing the field.

Metrics

Metrics

Download statistics
Download count
1
SciVal
FWCI
1.70
SciVal
Author count
6
SciVal
Paper percentile
84
SciVal
citations
14
Scopus
citations
14

PlumX, opens in new tab

Captures
38
Citation count
14