Due to their soft and brittle nature, the mechanical characterization of polymer hydrogels is a difficult task employing traditional testing equipment. Here, we endowed poly(N-isopropyl acrylamide) (PNIPAAm) hydrogel networks with Diels–Alder adducts of π-extended anthracenes as mechanofluorophore crosslinkers. After swelling the networks with varying amounts of water and subjecting them to force, we visualized the subsequent fluorescence caused by covalent bond scission with confocal laser scanning microscopy (CLSM) and related the intensities to the macroscopic fracture mechanics and the elastic moduli recorded with traditional uniaxial compression. The sensitivity of the mechanofluorophores allowed the analysis of low levels of mechanical stress produced via a hand-induced needle-puncturing process and, thus, is an alternative to conventional force application methods. The detection and precise localization of covalent bond scission via CLSM helps elucidating the interrelationship between molecular structure and the macroscopic properties of chemically crosslinked polymeric hydrogels. We believe that this micro-scale mechanophore-assisted fractography can establish a new paradigm for the mechanical analysis of soft matter in fields covering traditional polymer and life sciences.
Originele taal-2Engels
Pagina's (van-tot)358-366
Aantal pagina's9
TijdschriftPolymer Chemistry
Volume11
Nummer van het tijdschrift2
Vroegere onlinedatum26 jul 2019
DOI's
StatusGepubliceerd - 14 jan 2020

Vingerafdruk

Fractography
Hydrogels
Covalent bonds
Hydrogel
Confocal Microscopy
Anthracenes
Microscopic examination
Polymers
Scanning
Equipment testing
Mechanical Stress
Piercing
Biological Science Disciplines
Lasers
Elastic Modulus
Molecular Structure
Mechanics
Fracture mechanics
Needles
Molecular structure

Citeer dit

@article{e06b40f6491b48daba5d9d0cedaec927,
title = "Fractography of poly(N-isopropylacrylamide) hydrogel networks crosslinked with mechanofluorophores using confocal laser scanning microscopy",
abstract = "Due to their soft and brittle nature, the mechanical characterization of polymer hydrogels is a difficult task employing traditional testing equipment. Here, we endowed poly(N-isopropyl acrylamide) (PNIPAAm) hydrogel networks with Diels–Alder adducts of π-extended anthracenes as mechanofluorophore crosslinkers. After swelling the networks with varying amounts of water and subjecting them to force, we visualized the subsequent fluorescence caused by covalent bond scission with confocal laser scanning microscopy (CLSM) and related the intensities to the macroscopic fracture mechanics and the elastic moduli recorded with traditional uniaxial compression. The sensitivity of the mechanofluorophores allowed the analysis of low levels of mechanical stress produced via a hand-induced needle-puncturing process and, thus, is an alternative to conventional force application methods. The detection and precise localization of covalent bond scission via CLSM helps elucidating the interrelationship between molecular structure and the macroscopic properties of chemically crosslinked polymeric hydrogels. We believe that this micro-scale mechanophore-assisted fractography can establish a new paradigm for the mechanical analysis of soft matter in fields covering traditional polymer and life sciences.",
author = "Maria Stratigaki and Christoph Baumann and {van Breemen}, Lambert and Hans Heuts and Rint Sijbesma and Robert G{\"o}stl",
year = "2020",
month = "1",
day = "14",
doi = "10.1039/C9PY00819E",
language = "English",
volume = "11",
pages = "358--366",
journal = "Polymer Chemistry",
issn = "1759-9954",
publisher = "Royal Society of Chemistry",
number = "2",

}

Fractography of poly(N-isopropylacrylamide) hydrogel networks crosslinked with mechanofluorophores using confocal laser scanning microscopy. / Stratigaki, Maria; Baumann, Christoph; van Breemen, Lambert; Heuts, Hans; Sijbesma, Rint (Corresponding author); Göstl, Robert (Corresponding author).

In: Polymer Chemistry, Vol. 11, Nr. 2, 14.01.2020, blz. 358-366.

Onderzoeksoutput: Bijdrage aan tijdschriftTijdschriftartikelAcademicpeer review

TY - JOUR

T1 - Fractography of poly(N-isopropylacrylamide) hydrogel networks crosslinked with mechanofluorophores using confocal laser scanning microscopy

AU - Stratigaki, Maria

AU - Baumann, Christoph

AU - van Breemen, Lambert

AU - Heuts, Hans

AU - Sijbesma, Rint

AU - Göstl, Robert

PY - 2020/1/14

Y1 - 2020/1/14

N2 - Due to their soft and brittle nature, the mechanical characterization of polymer hydrogels is a difficult task employing traditional testing equipment. Here, we endowed poly(N-isopropyl acrylamide) (PNIPAAm) hydrogel networks with Diels–Alder adducts of π-extended anthracenes as mechanofluorophore crosslinkers. After swelling the networks with varying amounts of water and subjecting them to force, we visualized the subsequent fluorescence caused by covalent bond scission with confocal laser scanning microscopy (CLSM) and related the intensities to the macroscopic fracture mechanics and the elastic moduli recorded with traditional uniaxial compression. The sensitivity of the mechanofluorophores allowed the analysis of low levels of mechanical stress produced via a hand-induced needle-puncturing process and, thus, is an alternative to conventional force application methods. The detection and precise localization of covalent bond scission via CLSM helps elucidating the interrelationship between molecular structure and the macroscopic properties of chemically crosslinked polymeric hydrogels. We believe that this micro-scale mechanophore-assisted fractography can establish a new paradigm for the mechanical analysis of soft matter in fields covering traditional polymer and life sciences.

AB - Due to their soft and brittle nature, the mechanical characterization of polymer hydrogels is a difficult task employing traditional testing equipment. Here, we endowed poly(N-isopropyl acrylamide) (PNIPAAm) hydrogel networks with Diels–Alder adducts of π-extended anthracenes as mechanofluorophore crosslinkers. After swelling the networks with varying amounts of water and subjecting them to force, we visualized the subsequent fluorescence caused by covalent bond scission with confocal laser scanning microscopy (CLSM) and related the intensities to the macroscopic fracture mechanics and the elastic moduli recorded with traditional uniaxial compression. The sensitivity of the mechanofluorophores allowed the analysis of low levels of mechanical stress produced via a hand-induced needle-puncturing process and, thus, is an alternative to conventional force application methods. The detection and precise localization of covalent bond scission via CLSM helps elucidating the interrelationship between molecular structure and the macroscopic properties of chemically crosslinked polymeric hydrogels. We believe that this micro-scale mechanophore-assisted fractography can establish a new paradigm for the mechanical analysis of soft matter in fields covering traditional polymer and life sciences.

UR - http://www.scopus.com/inward/record.url?scp=85077541073&partnerID=8YFLogxK

U2 - 10.1039/C9PY00819E

DO - 10.1039/C9PY00819E

M3 - Article

VL - 11

SP - 358

EP - 366

JO - Polymer Chemistry

JF - Polymer Chemistry

SN - 1759-9954

IS - 2

ER -