Experimental characterization of ductile damage using nanoindentation

Onderzoeksoutput: Hoofdstuk in Boek/Rapport/CongresprocedureConferentiebijdrageAcademicpeer review

1 Downloads (Pure)

Samenvatting

In most types of sheet metal forming processes, such as drawing, stretching and bending operations, necking is the primary limiting factor in defining safe forming regions. However, it is also observed that, material failure can occur without any significant neck formation especially for non-traditional materials with relatively low formability, such as some aluminum alloys and high strength steels, [1]. The mechanisms of such failures are not very clearly identified but it is believed that internal damage is an important parameter in these occurrences (Fig. 1).
Originele taal-2Engels
TitelExperimental analysis of nano and engineering materials and structures : Proceedings of the 13th international conference on experimental mechanics, 1-6 July 2007, Alexandroupolis, Greece
RedacteurenE.E. Gdoutos
Plaats van productieGreece, Alexandroupolis
Pagina's149-150
DOI's
StatusGepubliceerd - 2007