Atomic layer deposition enabled perovskite/PEDOT solar cells in a regular n-i-p architectural design

D. Koushik, W.J.H. Verhees, Dong Zhang, Y. Kuang, S. Veenstra, M. Creatore, R.E.I. Schropp

Onderzoeksoutput: Bijdrage aan tijdschriftTijdschriftartikelAcademicpeer review

23 Citaten (Scopus)
1 Downloads (Pure)

Samenvatting

Perovskite solar cells employing poly(3,4-ethylenedioxythiophene) (PEDOT) as hole transport layer on top of methylammonium lead halide are reported, yielding a power conversion efficiency of 11% and a 6% stabilized power output. An atomic layer deposition assisted interface architectural approach is adopted to fabricate the n–i–p perovskite/PEDOT devices. The results present a promising next step toward efficient low-cost perovskite-based photovoltaic technology.
Originele taal-2Engels
Artikelnummer1700043
Aantal pagina's7
TijdschriftAdvanced Materials Interfaces
Volume4
Nummer van het tijdschrift18
Vroegere onlinedatum21 mrt 2017
DOI's
StatusGepubliceerd - 22 sep 2017

Vingerafdruk

Duik in de onderzoeksthema's van 'Atomic layer deposition enabled perovskite/PEDOT solar cells in a regular n-i-p architectural design'. Samen vormen ze een unieke vingerafdruk.

Citeer dit