Abstract
The recovery occurs in 4 stages; (I) below -10 Deg (recovery 14% Dr0), (II) -10 to +90 Deg, (III) 180 to 300 Deg (recovery .apprx.40% Dr0), and (IV) 300 to 580 Deg (recovery .apprx.24% Dr0). Stage I V is due to diffusion of simple vacancies. The activation energy of Pt.in stage III is a const. at 0.66 +- 0.06 e.v. from -30 Deg to +70 Deg. The recovery behaviors of Pt and Rh are essentially the same, and different from Cu. [on SciFinder (R)]