Method and apparatus for atomic layer deposition using an atmospheric pressure glow discharge plasma

H.W. Vries, de (Inventor), M.C.M. Sanden, van de (Inventor), M. Creatore (Inventor), W.M.M. Kessels (Inventor)

Research output: PatentPatent publication

Fingerprint

Dive into the research topics of 'Method and apparatus for atomic layer deposition using an atmospheric pressure glow discharge plasma'. Together they form a unique fingerprint.