Abstract
In carbon-supported Fe-Mo catalysts an Fe-Mo alloy can be formed during reduction in H2 at 673 K. In carbon-supported Co-Mo catalysts, instead of the formation of a Co-Mo alloy segregation of metallic Co is observed. In alumina-supported Fe and Fe-Mo catalysts, the interaction between the alumina support and the catalyst particles hinders reduction of the ions to an Fe0 phase. Most probably a surface "Fe(II)-aluminate" is formed.