Fracture behaviour and fractography of MnZn ferrites

M.A.H. Donners, L.J.M.G. Dortmans, G. With, de, M.J.M. Graaf, de

Research output: Chapter in Book/Report/Conference proceedingConference contributionAcademicpeer-review

Original languageEnglish
Title of host publicationProceeding of International Conference FRACTOGRAPHY '97
EditorsL. L'Parilak
Place of PublicationKosice, Slovakia
PublisherIMR SAS Kosice, Slovakia
Publication statusPublished - 1997

Cite this

Donners, M. A. H., Dortmans, L. J. M. G., With, de, G., & Graaf, de, M. J. M. (1997). Fracture behaviour and fractography of MnZn ferrites. In L. L'Parilak (Ed.), Proceeding of International Conference FRACTOGRAPHY '97 Kosice, Slovakia: IMR SAS Kosice, Slovakia.
Donners, M.A.H. ; Dortmans, L.J.M.G. ; With, de, G. ; Graaf, de, M.J.M. / Fracture behaviour and fractography of MnZn ferrites. Proceeding of International Conference FRACTOGRAPHY '97. editor / L. L'Parilak. Kosice, Slovakia : IMR SAS Kosice, Slovakia, 1997.
@inproceedings{78bff47b0eac4b8fa884f5a27f7c4a19,
title = "Fracture behaviour and fractography of MnZn ferrites",
author = "M.A.H. Donners and L.J.M.G. Dortmans and {With, de}, G. and {Graaf, de}, M.J.M.",
year = "1997",
language = "English",
editor = "L. L'Parilak",
booktitle = "Proceeding of International Conference FRACTOGRAPHY '97",
publisher = "IMR SAS Kosice, Slovakia",

}

Donners, MAH, Dortmans, LJMG, With, de, G & Graaf, de, MJM 1997, Fracture behaviour and fractography of MnZn ferrites. in L L'Parilak (ed.), Proceeding of International Conference FRACTOGRAPHY '97. IMR SAS Kosice, Slovakia, Kosice, Slovakia.

Fracture behaviour and fractography of MnZn ferrites. / Donners, M.A.H.; Dortmans, L.J.M.G.; With, de, G.; Graaf, de, M.J.M.

Proceeding of International Conference FRACTOGRAPHY '97. ed. / L. L'Parilak. Kosice, Slovakia : IMR SAS Kosice, Slovakia, 1997.

Research output: Chapter in Book/Report/Conference proceedingConference contributionAcademicpeer-review

TY - GEN

T1 - Fracture behaviour and fractography of MnZn ferrites

AU - Donners, M.A.H.

AU - Dortmans, L.J.M.G.

AU - With, de, G.

AU - Graaf, de, M.J.M.

PY - 1997

Y1 - 1997

M3 - Conference contribution

BT - Proceeding of International Conference FRACTOGRAPHY '97

A2 - L'Parilak, L.

PB - IMR SAS Kosice, Slovakia

CY - Kosice, Slovakia

ER -

Donners MAH, Dortmans LJMG, With, de G, Graaf, de MJM. Fracture behaviour and fractography of MnZn ferrites. In L'Parilak L, editor, Proceeding of International Conference FRACTOGRAPHY '97. Kosice, Slovakia: IMR SAS Kosice, Slovakia. 1997