Skip to main navigation Skip to search Skip to main content

Fouling behavior during microfiltration of silica nanoparticles and polymeric stabilizers

  • K.W. Trzaskus
  • , A. Zdeb
  • , W.M. de Vos
  • , A. Kemperman
  • , K. Nijmeijer

    Research output: Contribution to journalArticleAcademicpeer-review

    1 Downloads (Pure)

    Abstract

    Nanotechnology applications give rise to new forms of water pollution, resulting in a need for reliable technologies that can remove nanoparticles from water. Membrane filtration is an obvious candidate. The tendency of nanoparticles to become instable in suspension and form aggregates strongly influences their filtration behavior. This experimental study investigated fouling and rejection during dead-end microfiltration of sterically stabilized nanoparticles. Polyvinylpyrrolidone (PVP) with different molecular weights at different concentrations was used as model steric stabilizer. The large difference between membrane pore size (~200 nm) and the size of the silica nanoparticles (25 nm) allowed a detailed investigation of the filtration process and fouling development. We characterized the feed solution with optical reflectometry, dynamic light scattering, zeta potential measurements and asymmetric flow field flow fractionation (AF4) combined with static light scattering. Subsequently, we looked at the influence of the steric stabilizer (PVP) on nanoparticle fouling development during pore blocking and cake filtration stages.

    Our work demonstrates that molecular mass, concentration of the steric stabilizer (PVP) and filtration pressure significantly influence pore blockage and cake filtration. Using a stabilizer with a lower molecular mass generally led to better stabilization of the nanoparticles and the stabilizer contributed less to the fouling. While higher concentrations of the stabilizer enhanced the stability of the nanoparticles, they also caused faster fouling development due to the higher total solute load. Stabilizer with a higher molecular mass was found to contribute more to pore blockage and lead to faster fouling development. Use of a higher transmembrane pressure resulted in compression of the filtration cake, resulting in improved nanoparticle rejection at the expense of permeability
    Original languageEnglish
    Pages (from-to)205-215
    JournalJournal of Membrane Science
    Volume505
    DOIs
    Publication statusPublished - 1 May 2016

    Fingerprint

    Dive into the research topics of 'Fouling behavior during microfiltration of silica nanoparticles and polymeric stabilizers'. Together they form a unique fingerprint.

    Cite this