Cation-assisted lattice improvement of highly siliceous ZSM-5 upon prolonged heat treatment

B. Kraushaar, J.W. Haan, de, L.J.M. Ven, van de, J.H.C. Hooff, van

Research output: Contribution to journalArticleAcademicpeer-review

153 Downloads (Pure)

Abstract

Prolonged heat treatment of highly siliceous, template-free ZSM-5 containing Na+ or K+ causes improvement of the lattice structure, migration of alkaline ions to the outer layers of the zeolite particles as shown by XPS and an increased isolation of = Si–ONa sites from = Si–OH sites, as shown by 29Si CP MAS NMR analyses of silylated products
Original languageEnglish
Pages (from-to)1523-1526
JournalChemistry Letters
Volume15
Issue number9
DOIs
Publication statusPublished - 1986