Atomic layer deposition of low-dimensional transition metal di-and tri-chalcogenides and their heterostructures

Research output: ThesisPhd Thesis 1 (Research TU/e / Graduation TU/e)

11 Downloads (Pure)
Original languageEnglish
QualificationDoctor of Philosophy
Awarding Institution
  • Applied Physics
Supervisors/Advisors
  • Bol, Ageeth A., Promotor
  • Kessels, W.M.M. (Erwin), Promotor
Award date12 Nov 2020
Place of PublicationEindhoven
Publisher
Print ISBNs978-90-386-5155-2
Publication statusPublished - 12 Nov 2020