A new Nanoindentation Protocol for identifying the elasticity of undamaged extracellular bone tissue

  • Irina Furin
  • , Maria Ioana Pastrama
  • , Hawraa Kariem
  • , Krzysztof W. Luczynski
  • , Olaf Lahayne
  • , Christian Hellmich (Corresponding author)

Research output: Contribution to journalArticleAcademicpeer-review

131 Downloads (Pure)

Abstract

While the quest for understanding and even mimicking biological tissue has propelled, over the last decades, more and more experimental activities at the micro and nanoscales, the appropriate evaluation and interpretation of respective test results has remained a formidable challenge. As a contribution to tackling this challenge, we here describe a new method for identifying, from nanoindentation, the elasticity of the undamaged extracellular bone matrix. The underlying premise is that the tested bovine bone sample is either initially damaged (i.e. exhibits micro-cracks a priori) or that such micro-cracks are actually induced by the nanoindentation process itself, or both. Then, (very many) indentations may relate to either an intact material phase (which is located sufficiently far away from micro-cracks), or to differently strongly damaged material phases. Corresponding elastic phase properties are identified from the statistical evaluation of the measured indentation moduli, through representation of their histogram as a weighted sum of Gaussian distribution functions. The resulting undamaged elastic modulus of bovine femoral extracellular bone matrix amounts to 31 GPa, a value agreeing strikingly well both with direct quasi-static modulus tests performed on SEM-FIB-produced micro-pillars (Luczynski et al., 2015), and with the predictions of a widely validated micromechanics model (Morin and Hellmich, 2014). Further confidence is gained through observing typical indentation imprints under Scanning Electron Microscopy (SEM), which actually confirms the existence of the two types of micro-cracks as described above.

Original languageEnglish
Pages (from-to)693-704
Number of pages12
JournalMRS Advances
Volume1
Issue number11
DOIs
Publication statusPublished - 1 Jan 2016
Externally publishedYes

Funding

Financial support through project ERC-StG-2010 MICROBONE, #257032, is gratefully acknowledged. The authors are also grateful for the support of Jelena Zivkovic, in the course of the preliminary SEM-nanoindentation tests. Her stay at TU Wien was made possible through a scholarship of KMM-VIN.

Keywords

  • bone
  • elastic properties
  • nano-indentation

Fingerprint

Dive into the research topics of 'A new Nanoindentation Protocol for identifying the elasticity of undamaged extracellular bone tissue'. Together they form a unique fingerprint.

Cite this